EONO3D PP-GF Glass Fiber PP Filament 700g,Up to 30% Lighter than PLA | 1.75mm,Matte Black,Low Water Absorption,Tough PP-GF Engineering Material for Drones, RC Parts and Chemical Fixtures
Is this a good price? Every Thursday we email the cheapest price per kg for each major material, plus our best buy of the week.
Product Details
- UP TO 30% LIGHTER THAN PLA - Glass-fiber reinforced PP-GF has a low density, so the same part weighs up to 30% less than PLA and up to 10% less than standard PP. Ideal for drone frames, RC aircraft and weight-sensitive fixtures where every gram counts
- LOW WATER ABSORPTION - PP-GF takes up very little moisture, so filament and prints stay dimensionally stable in humid workshops and resist swelling, warping and strength loss. Dry 8 hours at 50°C after long storage for the best surface finish
- IMPACT TOUGH & FATIGUE RESISTANT - PP-GF absorbs heavy impacts through micro-deformation instead of cracking, and keeps its shape under repeated stress. Ideal for drone frames, RC bumpers, bike mudguards, hinges, brackets, jigs and fixing fixtures
- CHEMICAL & CORROSION RESISTANT - With strong interlayer adhesion, this polypropylene filament resists acids, alkalis and many solvents. Use it for pump bodies, valves, pipe fittings, plating tank liners, wastewater parts, spray nozzles and sensor housings
- EASY TO PRINT, LESS WARPING - 1.75mm ±0.03mm, 700g spool with stable diameter for smooth feeding. Print at 220-250°C with an 80-100°C bed, PP glue or tape and a hardened nozzle; reseal after use. Contains glass fiber: not for skin-contact or food-use parts
From the listing on Amazon.
View our other EONO3D listings here.
View our other PP-GF listings here.
Keep your filament dry, view our gear here.
Printing EONO3D PP-GF
EONO3D PP-GF in Matte Black is PP filled with chopped glass fiber, and this listing is a 0.7kg spool. The fibers make parts stiffer and more dimensionally stable than plain PP, but they are abrasive, so a hardened nozzle is mandatory (see nozzle compatibility below). Few makers publish separate PP-GF settings, so the ranges below are for plain PP; expect to print toward the top of them. Brands and even individual spools vary, so treat these as starting points and run a quick temperature tower to lock in the sweet spot for your printer.
Ranges checked against Prusa and Fiberlogy data. Heat resistance is the heat deflection temperature (HDT). Read our PP filament guide for bed adhesion, drying, troubleshooting, and material-specific tips.
Nozzle Compatibility
Glass fiber is abrasive and wears brass (and stainless) nozzles out of round, sometimes within a single spool. Use hardened steel or another wear resistant nozzle such as ruby or tungsten carbide. With hardened steel, start about 5 to 10°C hotter than you would with brass.